HAW-W06 soft rubber
HAW-W06 is a self vulcanizing soft rubber based on bromobutyl filled with carbon black, which can also be applied and vulcanized on site.
Description
HAW-W06 is a self vulcanizing soft rubber based on bromobutyl filled with carbon black, which can also be applied and vulcanized on site. The layer thickness of the rubber sheet may range between 3 and 6 mm.
Range of application
- Protective lining for structural components made of steel that are subjected to chemical exposure
- The lining of flue gas scrubbers for power plants and waste incineration, phosphoric acid plants, storage tanks, reaction vessels and pipes.
Characteristics
- an outstanding chemical resistance
- a high diffusion resistance
Chemical resistance
Resistant
- alkaline and acids
- oxidizing agents at lower and medium concentrations
- polar solvents
Limited resistance
None listed
Not resistant
- aromatics and greases
As listed on the data sheet. A medium not listed is untested, not unsuitable. Ask us about your exact medium and concentration.
Physical data
| Property | Value | Unit | Standard |
|---|---|---|---|
| Hardness | 65 ± 5 | Shore A | DIN 53505 |
| Specific weight | 1,21 ± 0,02 | g/cm³ | DIN EN ISO 1183 |
| Tensile strength* | ≥ 4 | MPa | DIN 53504 |
| Elongation at break* | > 300 | % | DIN 53504 |
| Rubber-metal-adhesion peeling test | ≥ 3 | N/mm | DIN EN 14879-4 |
| Max. service temperature | 100 | °C |
* values determined at 4 mm thick rubber samples
Processing notes
- The spark test (holiday test) of rubber lining is carried out according EN 14879-4 by using a high voltage tester. For carrying out the spark test, only the high voltage testers of the company Elmed model Isotest IIRT or Isotest Inspect 35 as well as the test pistols of company Wegener model WEG 20, WEG 22 or WEG 100 are allowed.